SBS static and fatigue tests were performed in Glare for two material orientations. SBS fatigue strength in longitudinal orientation was higher than in transversal. Longitudinal specimens presented interlaminar damage and cracks in middle span. Transversal specimens presented diverse failure modes at different τa levels. SBS test was considered adequate for both fatigue and static tests.