Durability of mortars made with sand washing waste
详细信息    查看全文
文摘

An industrial waste emanating from sand washing, rich in kaolinite, is used as a pozzolanic material.

Durability of mortars containing 0%, 10% and 30% of calcined waste is carried out in water, in HCl and Na2SO4 solutions.

Durability of mortars is evaluated by weight loss, expansion test, compressive strength and XRD analyses.

In the HCl solution, the decalcification of Csingle bondSsingle bondH and the dissolution of portlandite are observed.

Sulfates react with portlandite to produce gypsum and expansive ettringite.