摘要
采用交流阻抗谱法和电化学动电位再活化法研究热处理制度对低镍铬锰氮奥氏体不锈钢晶间腐蚀敏感性的影响。结果表明:在550~750℃范围内,晶间腐蚀敏感性随着温度的升高和保温时间的延长而增强。950℃热处理试样无腐蚀倾向。
Effect of heat treatment processes on intergranular corrosion sensitivity of low Ni-Cr-Mn-N austenitic stainless steel was investigated by means of double-loop electrochemical potentiokinetic reaction( DL-EPR) and electrochemical impedance spectroscopy( EIS)methods. The results show that at range of 550-750 ℃,with the prolongation of heating temperature and holding time,the sensitivity of intergranular corrosion rises. And the specimen treated at 950 ℃ has no intergranular corrosion.
引文
[1]边娜.晶间腐蚀定量化表示方法研究[D].保定:华北电力大学,2008.Bian Na.The research of intercry stalline corrosion quantitative expression method[D].Baoding:North China Electric Power University,2008.
[2]乌日根,董俊慧,朱霞.耐碱蚀稀土合金铸铁研究与发展概述[J].稀土,2006,27(6):83-85.Wu Rigen,Dong Junhui,Zhu Xia.Summary of research and development on alkali corrosion resistant alloy cast iron containing rare earths[J].Chinese Rare Earths,2006,27(6):83-85.
[3]陈勇,邱绍宇,任江涛.热处理对0Cr18Ni11Ti热轧钢板及焊接接头性能的影响[J].金属热处理,2003,28(7):23-26.Chen Yong,Qin Shaoyu,Ren Jiangtao.Effect of heat treatment on property of hot-rolled steel plate and welding joint of 0Cr18Ni11Ti steel[J].Heat Treatment of Metals,2003,28(7):23-26.
[4]杨胜,易丹青,姚素娟.热处理对2E12铝合金耐腐蚀性及力学性能的影响[J].金属热处理,2007,32(9):9-13.Yang Sheng,Yi Danqing,Yao Sujuan.Effect of heat treatment on corrosion resistance and mechanical properties of 2E12 aluminum alloy[J].Heat Treatment of Metals,2007,32(9):9-13.
[5]方智,张玉林,吴荫顺.电化学动电位再活化法评价308L不锈钢的晶间腐蚀敏感性[J].腐蚀科学与防护技术,1996,8(2):87-93.Fang Zhi,Zhang Yulin,Wu Yinshun.Detecting susceptibility to intergranular corrosion of 308L stainless steel by EPR method[J].Journal of the Chinese Society for Corrosion and Protection,1996,8(2):87-93.
[6]高中平,陈范才,赵常就.EPR法评价不锈钢晶间腐蚀敏感性的各种判据的比较[J].中国腐蚀与防护学报,2000,20(4):243-247.Gao Zhong ping,Chen Fancai,Zhao Changjiu.Different criteria of EPR method evaluate the susceptibility to intergranular corrosion[J].Journal of the Chinese Society for Corrosion and Protection,2000,20(4):243-247.
[7]武晋花.用电化学方法测量不锈钢晶间腐蚀的敏感性[J].冶金标准化与测量,2001,39(3):12-14.Wu Jinhua.Using electrochemical reactivation method survey stainless steel grain-boundary corrosion sensitivity[J].Metallurgical Standardization&Quality,2001,39(3):12-14.
[8]刘贵立,李荣德.稀土及杂质元素对ZA27合金晶间腐蚀的影响[J].化学物理学报,2004,17(5):649-651.Liu Guili,Li Rongde.Influence of RE and impurity element on the intergranular corrosion of ZA27 alloys[J].Chinese Journey of Chemical Physics,2004,17(5):649-651.
[9]Huang C A,Chang Y Z,Chen S C.The electrochemical behavior of austenitic stainless steel with different degrees of sensitization in the transpassive potential region in 1 mol/L H2SO4containing chloride[J].Corrosion Science,2004,46:1501-1513.
[10]秦丽雁,宋诗哲,卢玉琢.304不锈钢晶间腐蚀过程中的电化学组抗谱特征[J].中国腐蚀与防护学报,2007,27(2):74-79.Qin Liyan,Song Shizhe,Lu Yuzhuo.EIS characteristics of 304 stailess steel during intergranular corrosion[J].Journal of the Chinese Society for Corrosion and Protection,2007,27(2):74-79.
[11]于晓飞.304、316不锈钢晶间腐蚀的实验与理论研究[D].山东:山东大学,2007.Yu Xiaofei.Study of the intergranular corrosion of stainless steel(304,316)by experimental and theotical methods[D].Shandong University,2007.
[12]范光伟,张寿禄,秦丽雁.304不锈钢晶间腐蚀发展过程的阻抗谱分析[J].试验研究,2007(3):12-15.Fan Guangwei,Zhang Shoulu,Qin Liyan.Electrochemical impedance spectroscopy of 304 stainless steels during intergranular corrosion[J].Research Studies on Foundry Equipment,2007(3):12-15.
[13]董方,赵晓辉,杨雷.铈对00Cr12晶间腐蚀影响的试验研究[J].稀土,2014,35(1):86-91.Dong Fang,Zhao Xiaohui,Yang Lei.Effect of Ce on intergranuler corrosion of 00Cr12 ferrite stainless steel[J].Chinese Rare Earths,2014,35(1):86-91.
[14]李劲风,曹发和,张昭.Al-Li合金在EXCO溶液中腐蚀的电化学阻抗研究[J].金属学报,2003,39(4):426-430.Li Jinfeng,Cao Fahe,Zhang Zhao.Study on electrochemical impedance features of Al-Li alloys in EXCO solution[J].Acta Metallurgica Simica,2003,39(4):426-430.